<gallery caption="The results of the nano1.0 recipe" widths="400" heights="350" perrow="2">
<gallery caption="The results of process B after 17 and 34 cycles of etching" heights="350" perrow="2">
image:Travkatesting1a.jpg|  
image:Travkatesting1a.jpg|  
image:Travkatesting1b.jpg|The 60 nm trenches
image:Travkatesting1b.jpg|The 60 nm trenches
</gallery>