Specific Process Knowledge/Back-end processing/Laser Micromachining Tool: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 1: | Line 1: | ||
The Laser Micromachining Tool is a microSTRUCT vario from the company 3D-Micromac AG. | The Laser Micromachining Tool is a microSTRUCT vario from the company 3D-Micromac AG. | ||
The system | It is currently only for use by Danchip personel for internal training. | ||
It will be public available some time during the first half year of 2013. | |||
The system is able to produce micro structures in different kinds of materials like metals, ceramics, composite materials, etc. | |||
The machine is located in the basement of building 346 under the cleanroom. | The machine is located in the basement of building 346 under the cleanroom. | ||
It is | It is equipped with 2 high power lasers: | ||
* a 50W picosecond laser that can emit light at 3 wavelengths: 355nm, 532nm and 1064nm and a | |||
* a 100W nanosecond laser with a wavelength of 1064nm. | |||
[[File:Laser_Micromachining_Tool_main_parts_drawing.jpg|400px|thumb|Lasertool microSTRUCT vario (3D-Micromac AG)]] | |||
It consist of these main parts: | It consist of these main parts: | ||
* Upper service way | |||
* Manual front door | |||
* Operating panel | |||
* Machine's feet (adjustable) | |||
* Left service way | |||
* Electrical cabinet | |||
Revision as of 10:27, 21 January 2013
The Laser Micromachining Tool is a microSTRUCT vario from the company 3D-Micromac AG.
It is currently only for use by Danchip personel for internal training. It will be public available some time during the first half year of 2013.
The system is able to produce micro structures in different kinds of materials like metals, ceramics, composite materials, etc.
The machine is located in the basement of building 346 under the cleanroom.
It is equipped with 2 high power lasers:
- a 50W picosecond laser that can emit light at 3 wavelengths: 355nm, 532nm and 1064nm and a
- a 100W nanosecond laser with a wavelength of 1064nm.

It consist of these main parts:
- Upper service way
- Manual front door
- Operating panel
- Machine's feet (adjustable)
- Left service way
- Electrical cabinet