Specific Process Knowledge/Characterization/SEM: Scanning Electron Microscopy: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 3: | Line 3: | ||
At the moment we have three SEM's. Together they cover a wide range of needs in the cleanroom: From the fast in-process verification of different process parameters such as etch rates, step coverages or lift-off quality to the ultra high resolution images on any type of sample intended for publication. | At the moment we have three SEM's. Together they cover a wide range of needs in the cleanroom: From the fast in-process verification of different process parameters such as etch rates, step coverages or lift-off quality to the ultra high resolution images on any type of sample intended for publication. | ||
The SEM that will cover most users needs is the [[/Leo|Leo SEM]]. It is a very reliable and rugged | The SEM that will cover most users needs is the [[/Leo|Leo SEM]]. It is a very reliable and rugged instrument that provides high quality images of most samples. Due to its robustness new users only need a mandatory two hour training session before they are free to use it by themselves. | ||
before they are free to use it by themselves. | |||
The [[/Leo|Leo SEM]] is a standard instrument with a field emission gun and 3 high vacuum detectors, the Se2, Inlens and RBSD. A Röntec | |||
==[[/FEI | FEI SEM]] - ''FEI Nova 600 NanoSEM'' == | ==[[/FEI | FEI SEM]] - ''FEI Nova 600 NanoSEM'' == | ||
Revision as of 18:06, 24 November 2007
The Scanning Electron Microscopes at Danchip
At the moment we have three SEM's. Together they cover a wide range of needs in the cleanroom: From the fast in-process verification of different process parameters such as etch rates, step coverages or lift-off quality to the ultra high resolution images on any type of sample intended for publication.
The SEM that will cover most users needs is the Leo SEM. It is a very reliable and rugged instrument that provides high quality images of most samples. Due to its robustness new users only need a mandatory two hour training session before they are free to use it by themselves.
The Leo SEM is a standard instrument with a field emission gun and 3 high vacuum detectors, the Se2, Inlens and RBSD. A Röntec