== Silicon etching on the ICP Metal Etcher ==
In the primary silicon etcher at Danchip, the DRIE-Pegasus, silicon is etched using a fluorine based plasma (with SF<sub>6<\sub> as etch gas). Silicon is also etched by chlorine and bromine.
*[[Specific Process Knowledge/Etch/ICP Metal Etcher/silicon/nano|Etch of nanostructures in silicon]]
*[[Specific Process Knowledge/Etch/ICP Metal Etcher/silicon/nano|Etch of nanostructures in silicon]]

Revision as of 14:12, 11 December 2012

Silicon etching on the ICP Metal Etcher

In the primary silicon etcher at Danchip, the DRIE-Pegasus, silicon is etched using a fluorine based plasma (with SF6<\sub> as etch gas). Silicon is also etched by chlorine and bromine.