Specific Process Knowledge/Characterization/SEM: Scanning Electron Microscopy: Difference between revisions
No edit summary |
|||
| Line 23: | Line 23: | ||
== Process information == | == Process information == | ||
*[[Specific Process Knowledge/Characterization/SEM|SEMming]] | *[[Specific Process Knowledge/Characterization/SEM|SEMming]] | ||
*[[Specific Process Knowledge/Characterization/SEM/Leo|The Leo SEM]] | |||
*[[Specific Process Knowledge/Characterization/SEM/Zeiss|The Zeiss SEM]] | |||
*[[Specific Process Knowledge/Characterization/SEM/FEI|The FEI SEM]] | |||
*[[Specific Process Knowledge/Characterization/SEM/Jeo|The Jeol SEM]] | |||
[[/FEI | FEI SEM]] - ''FEI Nova 600 NanoSEM'' | |||
[[/Leo | Leo SEM]] - ''Leo 1550 '' | |||
[[/Jeol | Jeol SEM]] - ''Jeol JSM 5500 LV '' | |||
[[/SEM: Scanning Electron Microscopy/Zeiss|Zeiss SEM]] | |||
==Equipment performance and process related parameters== | ==Equipment performance and process related parameters== | ||
| Line 189: | Line 205: | ||
|- | |- | ||
|} | |} | ||
Revision as of 10:40, 3 December 2012



Scanning electron microscopy at Danchip
The four SEM's at Danchip cover a wide range of needs both in the cleanroom and outside: From the fast in-process verification of different process parameters such as etch rates, step coverages or lift-off quality to the ultra high resolution images on any type of sample intended for publication.
The 'workhorse' SEM that will cover most users needs is the Leo SEM. It is a very reliable and rugged instrument that provides high quality images of most samples. Excellent images on a large variety of materials such as semiconductors, semiconductor oxides or nitrides, metals, thin films and some polymers may be acquired on the Leo SEM. As such, we prefer that new users that have no prior SEM experience get trained on the Leo SEM before they start using the FEI or Zeiss.
The Zeiss SEM is the newest SEM in the cleanroom. It's a state-of-the-art SEM that will produce excellent images on almost any sample. Operated by the same user interface as the Leo, it is quite straight forward to change between the two instruments.
The FEI SEM was acquired to cope with the growing need for polymer related imaging. It is a versatile microscope with two vacuum modes (High Vacuum and Low Vacuum) and 6 different detectors, offering excellent resolution on any type of sample or material. This great performance, however, requires a skilled operator that knows how to achieve it. Also, we have learned that the high degree of sophistication and the great number of detectors make it much less robust compared to the other SEM's. It is therefore the intention that only users with special needs (for instance thick polymers, glass substrates or EDX/micromanipulator experiments) that will be trained. Furthermore, the instrument is equipped with a Oxford Inca EDX system and a Kleindiek micromanipulator with a Capres 4 point probe.
Outside the cleanroom in the basement of building 347, the Jeol SEM provides a possibilty of imaging samples that do not go into the cleanroom.
The user manuals, quality control procedures and results, user APVs, technical information and contact information can be found in LabManager:
- The SEM Leo page in LabManager,
- The SEM FEI page in LabManager,
- The SEM Zeiss page in LabManager,
- The SEM Jeol page in LabManager,
Process information
FEI SEM - FEI Nova 600 NanoSEM
Leo SEM - Leo 1550
Jeol SEM - Jeol JSM 5500 LV
| Equipment | SEM Leo | SEM Zeiss | SEM FEI | SEM Jeol | |
|---|---|---|---|---|---|
| Purpose | Imaging |
|
|
|
|
| Performance | Resolution |
|
|
|
|
| Optimum usage |
|
|
|
| |
| Process parameter range | Detectors |
|
|
|
|
| Stage |
|
|
|
| |
| Electron source |
|
|
|
| |
| Operating pressures |
|
|
|
| |
| Substrates | Sample sizes |
|
|
|
|
| Allowed materials |
|
|
|
| |
| SEM - Zeiss | SEM - FEI | SEM - Leo | SEM - Jeol | |
|---|---|---|---|---|
| Model | Zeiss Supra 55 VP | FEI Nova 600 NanoSEM | Leo 1550 SEM | Jeol JSM 5500 LV SEM |
| Substrate size | Up to 6" wafer with full view | Up to 6" wafer with 4" full view | Up to 4" wafer with full view | |
| Additional equipment | Kleindiek micromanipulator with Capres 4 point probe | |||
| EDX analysis | Oxford Inca system | Röntec system | Not available |