Specific Process Knowledge/Thermal Process/BCB Curing Oven: Difference between revisions
Appearance
No edit summary |
|||
| Line 1: | Line 1: | ||
== BCB Curing Oven == | == BCB Curing Oven == | ||
Revision as of 09:58, 3 December 2012
BCB Curing Oven
The BCB Curing Oven is mainly used for curing of BCB (bisbenzocyclobutene) and for alloying of metal in a nitrogen atmosphere.
During processing the furnace is rapidly heated by use of five halogen lamps below the sample. The furnace is purged with a high or a low nitrogen flow. Samples are processed at atmospheric pressure or at vacuum
The user manual, user APV, technical information and contact information can be found in LabManager:

Process information
There are no standard processes on the furnace.
| Equipment | BCB Curing Oven | |
|---|---|---|
| Purpose |
| |
| Process parameter range | Temperature |
|
| Nitrogen flows |
| |
| Substrates | Batch size |
|
| Allowed materials
Use the right carrier wafer |
| |