Specific Process Knowledge/Characterization/Four-Point Probe: Difference between revisions
Line 39: | Line 39: | ||
| style="background:LightGrey; color:black"|Substrate material allowed | | style="background:LightGrey; color:black"|Substrate material allowed | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
*Silicon wafers | *Silicon wafers | ||
|- | |- | ||
|} | |} |
Revision as of 12:37, 29 November 2012
Four-Point Probe
The Four-Point Probe is a Veeco FPP-5000 for I/V measurement. The main purpose it to measure resistance and resistivity on a 4" silicon wafer. But can also be used to find thickness of thin layers or test if is a N- or P-type wafer.
The wafer are pushed down on the four pins so a measurement is performed. It works only for 4" wafers because a special holder is need.

The user manual,technical information and contact information can be found in LabManager:
Purpose | Resistance and resistivity measurement | |
---|---|---|
Performance | ||
Process parameter range | Process Temperature |
|
Process pressure |
| |
Substrates | Batch size |
|
Substrate material allowed |
|