The 4-Point Probe is used to make I/V measurement for resistance and resistivity measurement. But can also be used to find thickness of a layer or test if is a N- or P-type wafer.
The 4-Point Probe is used to make I/V measurement for resistance and resistivity measurement. But can also be used to find thickness of thin layers or test if is a N- or P-type wafer.

Revision as of 17:08, 28 November 2012

4-Point Probe

The 4-Point Probe is used to make I/V measurement for resistance and resistivity measurement. But can also be used to find thickness of thin layers or test if is a N- or P-type wafer.