Specific Process Knowledge/Thin film deposition/Deposition of Gold: Difference between revisions
Appearance
New page: Titanium can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment. {| border="1" cellspacing="0" cellpadding="4" ! ! E-beam evapora... |
No edit summary |
||
| Line 1: | Line 1: | ||
Gold can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment. | |||