==When the deposition is on one side of the wafer==
==When the deposition is on one side of the wafer==
#Measure the wafer bow on one of the profilometers (Tencor or Dektak 8). Save the measurement. It is a good idea to measure across most of the wafer in two directions perpendicular to each other.
#Measure the wafer bow on one of the profilometers (Dektak XTA_new or Dektak 8). Save the measurement. It is a good idea to measure across most of the wafer in two directions perpendicular to each other.
#Deposite the thin film
#Deposite the thin film
#Measure the wafer bow again:  
#Measure the wafer bow again: