Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300/IBE magnetic stack etch: Difference between revisions
Appearance
| Line 49: | Line 49: | ||
===Endpoint detection with SIMS=== | ===Endpoint detection with SIMS=== | ||
[[image:SIMS_end_point_detection.png|300x300px|thumb| | [[image:SIMS_end_point_detection.png|300x300px|thumb|left|The endpoint for etching is determined by the integrated SIMS]] | ||
End point detection is achieved by SIMS, and the etch rate is approximately 25 Nm/min. | End point detection is achieved by SIMS, and the etch rate is approximately 25 Nm/min. | ||
Resist stripping can be hard due to burned resist, to remedy this try to lover the current. Changing the currect will chance the sidewall angle and new studies of etch profiles will be necessary. For help, discussion and further info please contact Kristian Hagsted Rasmussen. | Resist stripping can be hard due to burned resist, to remedy this try to lover the current. Changing the currect will chance the sidewall angle and new studies of etch profiles will be necessary. For help, discussion and further info please contact Kristian Hagsted Rasmussen. | ||