Line 74: Line 74:
#With Interferometric objective 50X DI: [[Media: Sensofar_A1_vsi_50xDI_SNR_with_increased_gain_and_contrast.pdf|See the results here
#With Interferometric objective 50X DI: [[Media: Sensofar_A1_vsi_50xDI_SNR_with_increased_gain_and_contrast.pdf|See the results here
]]
]]
====Setting for no. 1====
Recipe: Trench
*Operation mode: trench
**+ Raw smoothing confocal
**+ fine shift
*Objective: EPI 100X-N
*Z scan
**Dual - bottom up
***top: 8µm
***Gap: 91µm
***Bottom: 8µm
**Speed factor: 1x
**+ Linear stage
*Threshold: 0.0%
*Light source
**Levels: 2
***900 -> 60
***Gain: default

Revision as of 11:56, 3 August 2012

Results from the Optical Profiler (Sensofar) acceptance test

The acceptance test was performed in January 2012 by STInstruments and Sensofar together with Pernille V. Larsen @ Danchip and Berit G. Herstrøm @ Danchip.

This Table shows the accpetance criteria

' Title Sample description / measurement Acceptance criteria
1 Patterned flat sample of silicon Sample material: Patterned silicon substrate. Depth 100±2 µm
Trench depth with aspect ratio 1:10 on a 10 µm wide trench
2 Patterned flat sample of silicon. Sample material: Patterned silicon substrate. Depth 91±2 µm
Trench depth with aspect ratio 1:11 on a 8 µm wide trench
3 Patterned flat sample of silicon Sample material: Patterned silicon substrate Depth 85±2 µm
Trench depth with aspect ratio 1:13 on a 6.4 µm wide trench
4 Patterned flat sample of glass 3D profile of pattern etched down in a quartz sample. Depth within ±1% from a standard profiler measurement and repeatability (3 successive measurements) within 0.1%
Pattern size 20 µm x 20 µm, depth 500 nm
5 Flat sample of silicon with thick patterned oxide Step height of patterned thick (10 µm) oxide on top of a silicon wafer. Step height must be within ±3% of a SEM profile measurement.
7 µm deep pattern, trench width 6 µm
6 Flat sample of silicon with thick layer of patterned polymer Sample material: SU8 on silicon. Height 69±2 µm
Pillar heights of 69 µm with 25 µm between pillar edges
7 Free standing structure Measure bow due to stress of a membrane. Membrane bow repeatability of 5 successive measurement within 2%
Membrane material: Si(2 µm)/SiO2(~1 µm)/Au(50 nm).
Membrane size: honey comb structure approximately 150 µm in diameter.
Bow < 500 nm
8 Stitching of large area Stitching 4 mm x 4 mm on same sample as in 7. The area consists of many closed packed honey comb formed membranes. Membrane bow must the same as on 7 within 2%
9 Narrow trenches and holes Sample material: Patterned silicon substrate. Depth 20±2 µm
2.5 µm wide trench in silicon with a depth of 20 µm
10 Film thickness measurement of transparent thin film Transparent thin film thickness of 28 nm SiO2 on Si SiO2 thickness 28±1 nm
11 Measurements of multiple stacks 120 nm nitride on 110 nm oxide on a silicon substrate Within ±2% on each layer from an ellipsometer measurement.
12 Film thickness measurements of transparent films on small structure Sample material: Si with 1.5 µm patterned AZ-resist Within ±1% from a standard profiler measurement.
Measure thickness of AZ-resist on pillars of 50 µm in diameter
13 Roughness repeatability Sample material: Si wafer with poly-silicon layer. Repeatability within 0.2%
3 successive measurements of the roughness

Results

Results of acceptance test no. 1

Sample material: Patterned silicon substrate Measurement: Trench depth with aspect ratio 1:10 on a 10 µm wide trench Acceptance criteria:Depth 100±2 µm

It was done in two ways:

  1. With confocal objective EPI 100x-N: See the results here
  2. With Interferometric objective 50X DI: See the results here

Setting for no. 1

Recipe: Trench

  • Operation mode: trench
    • + Raw smoothing confocal
    • + fine shift
  • Objective: EPI 100X-N
  • Z scan
    • Dual - bottom up
      • top: 8µm
      • Gap: 91µm
      • Bottom: 8µm
    • Speed factor: 1x
    • + Linear stage
  • Threshold: 0.0%
  • Light source
    • Levels: 2
      • 900 -> 60
      • Gain: default