===Elemental composition===
===Elemental composition===
[[image:Overview spectra Labadvisor.JPG|380x380px|left|thumb|XPS spectrum of a sample consisting of the elements silicon, oxygen and carbon.]]
[[image:Overview spectra Labadvisor.JPG|420x420px|left|thumb|XPS spectrum of a sample consisting of the elements silicon, oxygen and carbon.]]




Line 41: Line 41:




[[image:Si spectra Labadvisor.JPG|380x380px|left|thumb|XPS Si2p spectrum of Si sample]]
[[image:Si spectra Labadvisor.JPG|420x420px|left|thumb|XPS Si2p spectrum of Si sample]]




Line 81: Line 81:
===Depth profiling===
===Depth profiling===


[[Image:Stochiometry 20110510.JPG|380x380px|left|thumb|Stochiometry as a function of film depth (etch time). The relationship between Cr and Ni is quite stabel through the film. Measurements done with XPS-ThermoScientific ]]
[[Image:Stochiometry 20110510.JPG|425x425px|left|thumb|Stochiometry as a function of film depth (etch time). The relationship between Cr and Ni is quite constant through the film. Measurements done with XPS-ThermoScientific ]]
 
The analysis is made on a choosen spot on the sample surface (detected with the system camera). The technique, is as written above, very surface sensitive and probes only the top nanometers og the sample.
 
With the ion beam gun on the system a etch of the sample can be done. The system measures the desired spectras, do a etch step and measures the again. A series of etch cycles can be set up, measuring the composition of the sample through at different depths.
 
 
 
 
 
 
 
 
 
 


The analysis is made on a chosen spot on the sample surface (detected with the system camera). The technique, is as written above, very surface sensitive and probes only the top nanometers of the sample.


With the ion beam gun on the system a etch of the sample can be done. The system measures the desired spectra, do a etch step and measures the again. A series of etch cycles can be set up, measuring the composition of the sample through at different depths.






'''Example: NiCr film'''


As an illustration, a figure to the left, shows an elemental analysis through a metallic film consisting of Ni and Cr. The metallic layer was about 70 nm thick, and the atomic percentage of Ni and Cr was measured through the layer. 


In the graph, you see the atomic % as a function of etch depth, and it is possible to detect that the relationship between Ni and Cr is fairly constant through the metallic film.





Revision as of 09:09, 18 October 2011

XPS-ThermoScientific

A X-ray Photoecectron Spectroscopy (XPS) system can be used at Danchip. The system is a Thermo K-Alpha system, and is found in LabManager under the name XPS-ThermoScientific.

Elemental analysis

The XPS technique can be used to do elemental analysis. A comparision about techniques and intsrumens used for elemental analysis at Danchip can be found on the page Element analysis.


XPS technique

XPS is a surface sensitive and non destructive technique used for analysis of the elemental composition. Only the outermost atomic layers (some nanometers) are probed, but with an ion etch there is the possibility to probe deeper laying layers.


In the XPS spectrometer system the probed samples are irradiated by photons with a specific energy, and the photoelectrons that leaves the sample are detected. The energy levels of the electrons are elemental specific, and by measuring the energy of the outgoing electrons, it is possible to detect which elements that are present in a sample.


The technique can be used for different purposes:


Elemental composition

XPS spectrum of a sample consisting of the elements silicon, oxygen and carbon.


Each element give a specific "finger-print" in the XPS spectrum. The electrons in the atoms have different binding energies for all elements, and when measuring a photoelectron spectrum over a wide range of energies, the main line from each element will be placed at a specific energy in the spectra.

Here is shown a spectra measured over the energy range 0-1350 eV, and characteristic lines from three elements (C,O and Si) are seen and indicated in the spectrum.

The instrument program can use this information to give an estimate of the sample composition, giving the atomic procentage of the different elements.






Chemical state

XPS Si2p spectrum of Si sample



















Depth profiling

Stochiometry as a function of film depth (etch time). The relationship between Cr and Ni is quite constant through the film. Measurements done with XPS-ThermoScientific

The analysis is made on a chosen spot on the sample surface (detected with the system camera). The technique, is as written above, very surface sensitive and probes only the top nanometers of the sample.

With the ion beam gun on the system a etch of the sample can be done. The system measures the desired spectra, do a etch step and measures the again. A series of etch cycles can be set up, measuring the composition of the sample through at different depths.


Example: NiCr film

As an illustration, a figure to the left, shows an elemental analysis through a metallic film consisting of Ni and Cr. The metallic layer was about 70 nm thick, and the atomic percentage of Ni and Cr was measured through the layer.

In the graph, you see the atomic % as a function of etch depth, and it is possible to detect that the relationship between Ni and Cr is fairly constant through the metallic film.




A rough overview of XPS-ThermoScientific characteristics

Purpose Chemical analysis
  • Probing elemental composition
  • Chemical state identification
  • Non destructive technique
  • Surface sensitive
  • Depth profiling possible by ion beam etch of sample
Performance Spot size Can be set between 30µm - 400µm
Probing depth Depending on probed element. Max probe depth lies within 10-200 Å.
Resolution Dependent on probed elements. Concentrations down to about 0,5 atomic % can in some cases be detected.
Charge compensation

Flood gun can be used for charge compensation of non conductive samples

Finding structures Choose measuring spot from camera image (magnified)
Depth profiling Purpose With ion beam etch the top layer of the material can be removed, to do a depth profiling
Ion beam size About 0,3x1 mm
Substrates Substrate size

Max 60x60 mm

Substrate thickness

Max height about 20 mm