'''All measurements on this page has been made by Nanolab staff.'''  
'''All measurements on this page has been made by Nanolab staff.'''  


[[index.php?title=Category:Equipment|Etch Wet Gold]]
[[Category:Equipment|Etch Wet Gold]]
[[index.php?title=Category:Etch (Wet) bath|Gold]]
[[Category:Etch (Wet) bath|Gold]]


Ething of Gold can be done either wet or dry. For wet etching please see below on this page. Dry etching can be done with [[Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300|IBE]] by sputtering with Ar ions.  
Ething of Gold can be done either wet or dry. For wet etching please see below on this page. Dry etching can be done with [[Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300|IBE]] by sputtering with Ar ions.