HighScore Plus is part of the software package supplied with the Malvern Panalytical Aeris benchtop Powder XRD. It is meant for advanced powder XRD data analysis.  
HighScore Plus is part of the software package supplied with the Malvern Panalytical Aeris benchtop Powder XRD. It is meant for advanced powder XRD data analysis.  


This software is available on the shared data analysis computer located in 346-904 just to the right of the XRD Powder. You can log onto this computer either directly when you are sitting in front of it or through remote desktop from your own computer. For more details on how to login remotely, please see [https://labmanager.dtu.dk/view_binary.php?fileId=6393 this note] in LabManager - requires login.
This software is available on the shared data analysis computer located in 346-904 just to the right of the XRD Powder. You can log onto this computer either directly when you are sitting in front of it or through remote access. For more details on how to login remotely, see the dedicated info file in [https://labmanager.dtu.dk/function.php?module=Machine&view=view&page_id=169 the Labmanager Equipment Info page for the XRD Powder] ''(requires login)'' on the Documents page under Technical Documents (Public Access). It's called "remote-access-Highscore-SLSII-DataViewer-XRDMP.txt".


==Using HighScore Plus==