Specific Process Knowledge/Back-end processing/PDMS Microfluidic: Difference between revisions
Appearance
| Line 53: | Line 53: | ||
==3D printing== | ==3D printing== | ||
'''Punching'''[[File:Manual puncher.jpg|thumb|Example of a 20 mm commercial puncher used to cut individual chips out of a PDMS microfluidic wafer]] | |||
==Cutting PDMS== | ==Cutting PDMS== | ||
[[File:PDMS through-hole methods.jpg|500px|thumb|center|Scanning Electron Microscopy (SEM) micrographs for comparison of methods to fabricate through-holes in PDMS ]] | |||
[[File:PDMS through-hole methods.jpg|thumb|center|Scanning Electron Microscopy (SEM) micrographs for comparison of methods to fabricate through-holes in PDMS ]] | |||
'''Laser ablation''' | '''Laser ablation''' | ||