Specific Process Knowledge/Back-end processing/PDMS Microfluidic: Difference between revisions
Appearance
| Line 57: | Line 57: | ||
'''Punching'''[[File:Manual puncher.jpg|thumb|Example of a 20 mm commercial puncher used to cut individual chips out of a PDMS microfluidic wafer]] | '''Punching'''[[File:Manual puncher.jpg|thumb|Example of a 20 mm commercial puncher used to cut individual chips out of a PDMS microfluidic wafer]] | ||
[[File:PDMS through-hole methods.jpg|thumb|center|Scanning Electron Microscopy (SEM) micrographs for comparison of methods to fabricate through-holes in PDMS ]] | |||
'''Laser ablation''' | '''Laser ablation''' | ||