In our Polyfablab, we have UV lithography, various additive methods, coating techniques, and imprinting techniques for polymer processing.
In our Polyfablab, we have UV lithography, various additive methods, coating techniques, and imprinting techniques for polymer processing.


==[[Specific_Process_Knowledge/Lithography/Lithography/UVLithography|UV lithography]]==
==[[Specific_Process_Knowledge/Lithography/UVLithography|UV lithography]]==
*[[Specific_Process_Knowledge/Lithography/UVExposure/aligner_MA6-1|Mask Aligner: MA6-1]]
*[[Specific_Process_Knowledge/Lithography/UVExposure/aligner_MA6-1|Mask Aligner: MA6-1]]
*[[Specific_Process_Knowledge/Lithography/UVExposure/aligner_MLA4|Maskless Aligner: μMLA-04]]
*[[Specific_Process_Knowledge/Lithography/UVExposure/aligner_MLA4|Maskless Aligner: μMLA-04]]

Revision as of 11:01, 8 July 2026

The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.

Feedback to this page: click here

THIS PAGE IS UNDER CONSTRUCTION

Polymer Processing

THIS PAGE IS UNDER CONSTRUCTION

Polymer processing involves transforming polymer resins into finished products with desired shapes, dimensions and performance characteristics. It combines the principles of polymer science, heat transfer, fluid mechanics, and manufacturing technology to produce a wide range of components for various applications. The processing conditions, such as temperature, pressure, and cooling rate, significantly influence the final properties of the polymer product.

There is a wide range of methods available to structure and modify polymers, though commonly done outside of a cleanroom, whereas some can be done inside a cleanroom.

Many polymer processing methods may require a mask or stamp or some kind, e.g., injection molding, hot embossing or nano imprint lithography. Some methods can be used to directly "write" into the material, e.g., laser ablation or micromilling. Other methods, like 3D printing or 2-photon polymerisation, are called additive methods as they create the structure by building up the polymer structure.

In our Polyfablab, we have UV lithography, various additive methods, coating techniques, and imprinting techniques for polymer processing.

UV lithography

Additive Methods

Coating

Imprinting

Microscopes

Plasma Cleaner


Polymer Processing

There is a wide range of methods available to structure and modify polymers, though commonly done outside of a cleanroom.

Many polymer processing methods may require a mask or stamp or some kind, f.ex. injection molding, hot embossing or nano imprint lithography. Some methods can be used to directly "write" into the material, f.ex. laser ablation or micromilling. Other methods, like 3D printing or 2-photon polymerization are called additive methods as they create the structure by a building up the polymer structure.

Choose Method of Polymer Processing


Specialized Processes:

  • 3D printing
  • 2-Photon Polymerization Lithography


Choose Material for Polymer Processing

  • Epoxy, e.g. SU-8
  • Thermoplastic, e.g. PMMA, Topas (COC), PS, PC, PP, PET, etc
  • Photo Resist, e.g. AZ resists