Jump to content

Specific Process Knowledge/Polymer Processing: Difference between revisions

From LabAdviser
Meenadh (talk | contribs)
Meenadh (talk | contribs)
No edit summary
Line 8: Line 8:
<span style="background:#FF2800">'''THIS PAGE IS UNDER CONSTRUCTION'''</span>
<span style="background:#FF2800">'''THIS PAGE IS UNDER CONSTRUCTION'''</span>


[[Parylene coater]]
==UV lithography==
*[[Specific_Process_Knowledge/Lithography/UVExposure/aligner_MA6-1|Link to Aligner: MA6-1]]
*[[Specific Process Knowledge/Lithography/NanoImprintLithography|Nano Imprint Lithography]]
*[[Specific Process Knowledge/Lithography/UVLithography|UV Lithography]]
*[[Specific_Process_Knowledge/Lithography/Coaters/labspin04]]
 
==Additive techniques==
*[[Specific_Process_Knowledge/Lithography/UVExposure/aligner_MA6-1|Link to Aligner: MA6-1]]
*[[Specific Process Knowledge/Lithography/NanoImprintLithography|Nano Imprint Lithography]]
*[[Specific Process Knowledge/Lithography/UVLithography|UV Lithography]]
*[[Specific_Process_Knowledge/Lithography/Coaters/labspin04]]


= Polymer Processing =
= Polymer Processing =

Revision as of 10:58, 29 June 2026

The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.

Feedback to this page: click here

THIS PAGE IS UNDER CONSTRUCTION

PolyFabLab

THIS PAGE IS UNDER CONSTRUCTION

UV lithography

Additive techniques

Polymer Processing

There is a wide range of methods available to structure and modify polymers, though commonly done outside of a cleanroom.

Many polymer processing methods may require a mask or stamp or some kind, f.ex. injection molding, hot embossing or nano imprint lithography. Some methods can be used to directly "write" into the material, f.ex. laser ablation or micromilling. Other methods, like 3D printing or 2-photon polymerization are called additive methods as they create the structure by a building up the polymer structure.

Choose Method of Polymer Processing


Specialized Processes:

  • 3D printing
  • 2-Photon Polymerization Lithography


Choose Material for Polymer Processing

  • Epoxy, e.g. SU-8
  • Thermoplastic, e.g. PMMA, Topas (COC), PS, PC, PP, PET, etc
  • Photo Resist, e.g. AZ resists