Specific Process Knowledge/Lithography/Pretreatment/Oven 250C: Difference between revisions
Appearance
| Line 1: | Line 1: | ||
=Oven 250C= | =Oven 250C= | ||
[[ | [[file:Oven_250_degrees_for_pretreatment_cr3.jpg|400px|thumb|Oven 250C for pretreatment in Cx-1]] | ||
The oven is typically used for dehydration pretreatment, of Si and glass substrates, to promote the resist adhesion. We recommend placing the wafers in a metal carrier in the oven for at least for 4 hours, or overnight, and spin coat resist on them as soon as possible after removing them from the oven. | The oven is typically used for dehydration pretreatment, of Si and glass substrates, to promote the resist adhesion. We recommend placing the wafers in a metal carrier in the oven for at least for 4 hours, or overnight, and spin coat resist on them as soon as possible after removing them from the oven. | ||