Specific Process Knowledge/Lithography/EBeamLithography/Nanobook: Difference between revisions
Appearance
| Line 59: | Line 59: | ||
{| style="border: none; border-spacing: 0; margin: 1em auto; text-align: center;" | {| style="border: none; border-spacing: 0; margin: 1em auto; text-align: center;" | ||
|- | |- | ||
| [[ | | [[File:MobyDickSEM2.tif|400px]] | ||
|- | |- | ||
| colspan="1" style="text-align:center;| | | colspan="1" style="text-align:center;| | ||
SEM image of a small fraction of the book. Letter line width is 31 nm and letter height is about 116 nm. | SEM image of a small fraction of the book. Letter line width is 31 nm and letter height is about 116 nm. | ||
|} | |} | ||