| Linewidth and sidewall angle vs. defocus value for 2µm AZ nLOF exposed in Aligner: Maskless 01 (MLA1) using dose 220mJ/cm<sup>2</sup> | | colspan="2" | Linewidth and sidewall angle vs. defocus value for 2µm AZ nLOF exposed in Aligner: Maskless 01 (MLA1) using dose 220mJ/cm<sup>2</sup> and Aligner: Maskless 02 (MLA2) using dose 450mJ/cm<sup>2</sup>, respectively. <br>Blue circles: Width of 2µm line. Orange Squares: Sidewall angle. | ||
|} | |} | ||