===Resist profile (sidewall angle and linewidth)=== | ===Resist profile (sidewall angle and linewidth)=== | ||
*SEM pictures to support graphs? | |||
[[Image:5214E_Linewidth vs dose.jpg|left|500px|thumb|Width of 2µm line vs. exposure dose for 1.5µm AZ 5214E. <br>Blue circles: Exposed on Aligner: MA6-2 in vacuum contact. <br>Orange Squares: Exposed on Aligner: Maskless 02 (MLA2) using defoc 2 (QC defoc=2).]] | [[Image:5214E_Linewidth vs dose.jpg|left|500px|thumb|Width of 2µm line vs. exposure dose for 1.5µm AZ 5214E. <br>Blue circles: Exposed on Aligner: MA6-2 in vacuum contact. <br>Orange Squares: Exposed on Aligner: Maskless 02 (MLA2) using defoc 2 (QC defoc=2).]] | ||