Created page with "=Plasma Asher 5= 400px|thumb|Plasma asher 5 in cleanroom E-5.|right Product name: PVA Tepla Gigabatch 380M<br> Year of purchase: 2024 The Plasma Asher 5 can be used for the following processes: *Photoresist stripping *Descumming *Surface cleaning *Removal of organic passivation layers and masks Furthermore plasma processing using CF<sub>4</sub> in plasma asher 5 can be used for: *Etching of glass and ceramic *Etching of SiO<sub>2</sub>, Si<sub>3..."
 
Jehem (talk | contribs)
 
Line 21: Line 21:
The user manual, risk assessment, and contact information can be found in [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=531 LabManager] - '''requires login'''
The user manual, risk assessment, and contact information can be found in [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=531 LabManager] - '''requires login'''


===Process Information===
==Process Information==
Plasma asher 5 is identical to plasma asher 4, see resist strip processing for plasma asher 4 [[Specific_Process_Knowledge/Lithography/Strip#Plasma_Asher_4|here]].
Plasma asher 5 is identical to plasma asher 4, see resist strip processing for plasma asher 4 [[Specific_Process_Knowledge/Lithography/Strip#Plasma_Asher_4|here]].



Latest revision as of 12:21, 12 January 2026

Plasma Asher 5

Plasma asher 5 in cleanroom E-5.

Product name: PVA Tepla Gigabatch 380M
Year of purchase: 2024

The Plasma Asher 5 can be used for the following processes:

  • Photoresist stripping
  • Descumming
  • Surface cleaning
  • Removal of organic passivation layers and masks


Furthermore plasma processing using CF4 in plasma asher 5 can be used for:

  • Etching of glass and ceramic
  • Etching of SiO2, Si3N4, Si
  • Removal of polyimide layers


Plasma asher 5 can be used for almost every material, but if you have any doubt if your materials are compatible/allowed in plasma asher 5, feel free to ask the lithography group at Nanolab.

The user manual, risk assessment, and contact information can be found in LabManager - requires login

Process Information

Plasma asher 5 is identical to plasma asher 4, see resist strip processing for plasma asher 4 here.


Processes specifically only for plasma asher 5: