Specific Process Knowledge/Lithography/Coaters/labspin04: Difference between revisions

From LabAdviser
Taran (talk | contribs)
Taran (talk | contribs)
 
Line 2: Line 2:
[[Image:Labspin_2.JPG|400px|thumb|Spin coater: LabSpin 04 is located in PolyFabLab in building 347]]
[[Image:Labspin_2.JPG|400px|thumb|Spin coater: LabSpin 04 is located in PolyFabLab in building 347]]


Spin Coater: LabSpin 04 is a model LabSpin6 TT spin coater from SUSS. It's primary purpose is spin coating of SU-8 resist. It was installed in PolyFabLab in 2024.
Spin Coater: LabSpin 04 is a model LabSpin6 TT spin coater from SUSS. It's primary purpose is spin coating of SU-8 resist. It was installed in PolyFabLab in 2025.


The user manual, user APV, and contact information can be found in [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=547 LabManager] - '''requires login'''
The user manual, user APV, and contact information can be found in [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=547 LabManager] - '''requires login'''

Latest revision as of 11:35, 3 November 2025

Spin Coater: LabSpin 04

Spin coater: LabSpin 04 is located in PolyFabLab in building 347

Spin Coater: LabSpin 04 is a model LabSpin6 TT spin coater from SUSS. It's primary purpose is spin coating of SU-8 resist. It was installed in PolyFabLab in 2025.

The user manual, user APV, and contact information can be found in LabManager - requires login

Training video (same tool in Cleanroom 346): LabSpin02 + 03

Process information

Useful information about resist dispense can be found here.

Equipment performance and process related parameters

Purpose
  • Spin coating of epoxy based resists
    • SU-8 series
    • SU-8 3000 series
    • SU-8 XFT series
    • mr-DWL series
  • Spin coating of other resists
Resist
  • manual dispense
Performance Coating thickness
  • SU-8 resists: 0.1-200 µm

Coating thickness range is dependent on specific resist formulation

Process parameters Spin speed

100 - 8000 rpm

Spin acceleration

200 - 4000 rpm/s (wrongly labelled 1/s^2 in the software)

Substrates Substrate size
  • chips, 5mm and up
  • 100 mm wafers
  • 150 mm wafers
Allowed materials

All PolyFabLab materials
See Cross Contamination Sheet in LabManager

Batch

1