Specific Process Knowledge/Lithography/Coaters/RCD8: Difference between revisions
Appearance
| Line 35: | Line 35: | ||
|style="background:LightGrey; color:black"|Coating thickness | |style="background:LightGrey; color:black"|Coating thickness | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
* SU-8 | * SU-8 resists: 0.1-200+ µm | ||
* AZ 5214E: 1.5-3 µm | * AZ 5214E: 1.5-3 µm | ||
* AZ 4562: 8-15 µm | * AZ 4562: 8-15 µm | ||
Latest revision as of 10:23, 3 November 2025
Spin Coater: RCD8

Spin Coater: RCD8 is a model RCD8 T spin coater from Süss MicroTec with a motorized media arm and Gyrset functionality. It's primary purpose is spin coating of SU-8 resist. The media arm was disabled in 2024.
However, due to the possibility of using a non-vacuum chuck, the spin coater is also suitable for coating of substrates with e.g. textured backsides or membranes.
The user manual, user APV, and contact information can be found in LabManager - requires login
Process information
| Purpose |
| |
|---|---|---|
| Resist |
| |
| Performance | Coating thickness |
|
| Process parameters | Spin speed |
Vacuum chuck: 10 - 5000 rpm |
| Spin acceleration |
10 - 3000 rpm/s | |
| Substrates | Substrate size |
|
| Allowed materials |
All cleanroom materials ? | |
| Batch |
1 |