Specific Process Knowledge/Lithography/Resist/UVresist: Difference between revisions
Appearance
| Line 284: | Line 284: | ||
'''New resists version in 2023'''<br> | '''New resists version in 2023'''<br> | ||
As of 2023-03-21 we no longer have any of the old versions of the resists: AZ 5214E, AZ 4562, AZ MiR 701. This table contains only information about the <i>old</i> resist versions. | As of 2023-03-21 we no longer have any of the old versions of the resists: AZ 5214E, AZ 4562, AZ MiR 701. <span style="color:red">This table contains only information about the <i>old</i> resist versions.</span> | ||
<br clear="all" /> | <br clear="all" /> | ||