Specific Process Knowledge/Thermal Process/Oxidation: Difference between revisions
Appearance
No edit summary |
|||
| Line 431: | Line 431: | ||
image:Oxide_thickness_vs_time_Dry_oxygen_111.JPG|Dry oxide on <111> wafer. The y-axis is in Å and the x-axis is in minutes. | image:Oxide_thickness_vs_time_Dry_oxygen_111.JPG|Dry oxide on <111> wafer. The y-axis is in Å and the x-axis is in minutes. | ||
</gallery> | </gallery> | ||
===Breakdown voltage measurements=== | ===Breakdown voltage measurements=== | ||