===Etching of | ===Etching of TiO2 using ICP metal has been tested Evgeniy Shkondin, DTU Nanolab=== | ||
Recipe used: Ti etch <br> | |||
[[image:TiO2_etch_Evgeniy2.jpg|400px]] | |||