|Etch rate of SiO2
|Etch rate of SiO2
|'''~42nm/min [41-43 nm/min over a 6" wafer]
|'''~42nm/min [41-43 nm/min over a 6" wafer]  
|'''13.7-14.7 nm/min [4" on carrier]
|'''13.7-14.7 nm/min [4" on carrier]