==Thermal deposition of Aluminium== | ==Thermal deposition of Aluminium== | ||
In the | In the Lesker Thermal evaporator aluminium can be deposited by thermal deposition. Some properties of the evaporated films are described on the following page: | ||
*[[/Thermal deposition of Al|Thermal deposition of Aluminium]] | *[[/Thermal deposition of Al|Thermal deposition of Aluminium]] | ||
==Comparison of Al deposition options== | ==Comparison of Al deposition options== | ||