Specific Process Knowledge/Thermal Process/C2 Furnace III-V oxidation: Difference between revisions
No edit summary |
No edit summary |
||
| Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:thinfilm@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process/C2_Furnace_III-V_oxidation click here]''' | '''Feedback to this page''': '''[mailto:thinfilm@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process/C2_Furnace_III-V_oxidation click here]''' | ||
''This page is written by DTU Nanolab | ''This page is written by DTU Nanolab internal'' | ||
==General Purpose Annealing furnace (C2) == | |||
==General Purpose Annealing furnace (C2)== | |||
The General Purpose Annealing furnace (C2) is a Tempress horizontal furnace located in the furnace C stack. | The General Purpose Annealing furnace (C2) is a Tempress horizontal furnace located in the furnace C stack. | ||
The | The furnace has from September 2024 become a general purpose annealing furnace. It means that it can be used for annealing of different samples and different materials, such as silicon substrates with metal layers. | ||
Annealings can be performed in a nitrogen atmosphere, with an nitrogen flow up to 10 SLM. | |||
An annealing temperature of maximum 600 C is allowed in the furnace, with a ramp rate of up to 10°C/min. The standby temperature is set to 250°C. | An annealing temperature of maximum 600 C is allowed in the furnace, with a ramp rate of up to 10°C/min. The standby temperature is set to 250°C. | ||
Samples must be able to tolerate the annealing temperature. A permission from the Thin Film group is also required, before samples are annealed in the furnace. | |||
Please also check the cross contamination information in LabManager, before you use the furnace. And note that samples that have been annealed in the furnace are considered "dirty" or "contaminated with metal traces" and are therefore not allowed in any other furnaces afterwards. | |||
4" wafers can be placed horizontally in a quartz boat in the furnace, and up to two 6" wafer can be placed horizontally on two boats. Small sample are placed on a 6" carrier wafer (with or without a recess) on a quartz boat. | |||
The furnace is | The motor for automatic opening and closing of furnace door is broken, and the door therefore has to be opened and closed manually. | ||
| Line 61: | Line 57: | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
*Up to 30 4" wafers | *Up to 30 4" wafers | ||
*1 6" wafers (placed horizontally on the | *1-2 6" wafers (placed horizontally on the boats) | ||
*Several smaller samples (placed horizontally on a 6" carrier wafer placed on the boat) | *Several smaller samples (placed horizontally on a 6" carrier wafer placed on the boat) | ||
|- | |- | ||
Revision as of 13:59, 27 May 2025
Feedback to this page: click here
This page is written by DTU Nanolab internal
General Purpose Annealing furnace (C2)
The General Purpose Annealing furnace (C2) is a Tempress horizontal furnace located in the furnace C stack.
The furnace has from September 2024 become a general purpose annealing furnace. It means that it can be used for annealing of different samples and different materials, such as silicon substrates with metal layers.
Annealings can be performed in a nitrogen atmosphere, with an nitrogen flow up to 10 SLM.
An annealing temperature of maximum 600 C is allowed in the furnace, with a ramp rate of up to 10°C/min. The standby temperature is set to 250°C.
Samples must be able to tolerate the annealing temperature. A permission from the Thin Film group is also required, before samples are annealed in the furnace.
Please also check the cross contamination information in LabManager, before you use the furnace. And note that samples that have been annealed in the furnace are considered "dirty" or "contaminated with metal traces" and are therefore not allowed in any other furnaces afterwards.
4" wafers can be placed horizontally in a quartz boat in the furnace, and up to two 6" wafer can be placed horizontally on two boats. Small sample are placed on a 6" carrier wafer (with or without a recess) on a quartz boat.
The motor for automatic opening and closing of furnace door is broken, and the door therefore has to be opened and closed manually.
The user manual and contact information can be found in LabManager:
General Purpose Annealing furnace (C2)
| Purpose |
| |
|---|---|---|
| Process parameter range | Annnealing temperature |
|
| Standby temperature |
| |
| Process pressure |
| |
| Gases on the system |
| |
| Substrates | Batch size |
|
| Substrate materials allowed |
|