The Rigaku 9kW Rotating Anode XRD SmartLab is an advanced XRD instrument for measuring thin films, powders, and other substances. All thin films can be measured without fixating the sample, as the system has a so called In-Plane arm.
The Rigaku SmartLab 9kW Rotating Anode XRD that we call "XRD Rot Anode" is an advanced XRD instrument for measuring thin films, powders, and other substances. All thin films can be measured without fixating the sample, as the system has a so called In-Plane arm.


[[image:eves_XRD_RotAnode_01.jpg|400x400px|right|thumb|The XRD SmartLab located in a basement 346-904]]
[[image:eves_XRD_RotAnode_01.jpg|400x400px|right|thumb|The XRD SmartLab located in a basement 346-904]]

Revision as of 15:20, 31 March 2025

Feedback to this page: click here

Unless otherwise stated, this page is written by DTU Nanolab internal
All images and photos on this page belongs to DTU Nanolab


XRD Rot Anode

The Rigaku SmartLab 9kW Rotating Anode XRD that we call "XRD Rot Anode" is an advanced XRD instrument for measuring thin films, powders, and other substances. All thin films can be measured without fixating the sample, as the system has a so called In-Plane arm.

The XRD SmartLab located in a basement 346-904


The user manual(s), user APV(s), technical information, and contact information can be found in LabManager:

XRD RotAnode SmartLab in LabManager - requires login


Various measurement types including X-Ray Reflectivity, Rocking Curve, Theta-2theta, and Pole figures are described here:

Process information


The measurement settings and results of the pre-acceptance test are described in this document, also found on the Lab Manager:

The same measurement were completed as part of the acceptance, but no report was generated. In addition the inspection certificate is available here: