Specific Process Knowledge/Back-end processing/Polishing machine: Difference between revisions
Appearance
No edit summary |
|||
| Line 6: | Line 6: | ||
'''All links Labmanager requires login.''' | '''All links Labmanager requires login.''' | ||
<big>''' Machine decommissioned end of 2024 ''' | |||
</big> | |||
== Polisher/Lapper == | == Polisher/Lapper == | ||
<big>''' Machine decommissioned end of 2024 ''' | |||
</big> | |||
<!-- copyright issue rkc --> | <!-- copyright issue rkc --> | ||
Revision as of 15:02, 30 January 2025
Feedback to this page: click here
Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.
All links Labmanager requires login.
Machine decommissioned end of 2024
Polisher/Lapper
Machine decommissioned end of 2024
The Logitech PM5 Polisher/Lapper is for thinning down wafers and other substrates.
The user manual, user APV, technical information and contact information can be found in LabManager:
The Logitech PM5 Polisher/Lapper in LabManager

| Equipment | Polisher/Lapper | |
|---|---|---|
| Purpose |
Thinning of substrates of |
|
| Performance | Thinning |
|
| Polishing |
| |
| Process parameter range | Polishing liquid |
|
| Polishing cloths |
| |
| Rotation speed |
| |
| Arm sweep |
| |
| Substrates | Batch size |
|
| Allowed materials |
| |