Etching of nanostructures in Si using DRIE-Pegasus: nano1.4 recipe, Run ID 2000, time 120 secs, SF6 38, C4F8 75, 4mtorr, 800/50 coil/platen, -20 degs.
 
Jml (talk | contribs)
uploaded a new version of "Image:WF 2E07a mar23 2011-030.jpg": Etching of nanostructures in Si using DRIE-Pegasus: nano1.4 recipe, Run ID 2000, time 120 secs, SF6 38, C4F8 75, 4mtorr, 800/50 coil/platen, -20 degs.
 