== Centrifuge 5430R ==
== Centrifuge 5430R ==
Specifications:
Two rotor are available for this centrifuge.
* Rotor FA-45-30-11
Allows max. capacity 30 micro test tubes for 1.5/
2.0 mL and operates at 25000 ×g /15350 rpm


* Rotor F-35-6-30
Allows max. capacity 6 conical tubes for 50 mL or 6 conical tubes for 15 mL and operates at 7745 ×g /7830 rpm
'''Specifications:'''
* Max. rotor capacity depending on type of rotor: 30 × 1.5/2.0 mL, 6 × 50 mL, 6 × 15 mL
* Max. speed: 25000 ×g (15350 rpm)
* Acceleration/braking time: <25/25 s
* Temperature range: -11 °C to +40 °C
* Run time: 30 s to 99:59 h, infinity