Jump to content

Specific Process Knowledge/Lithography/EBeamLithography/AR-P 617: Difference between revisions

Thope (talk | contribs)
Thope (talk | contribs)
Line 22: Line 22:


=Contrast curve=
=Contrast curve=
A contrast curve for AR-P 617.06 is provided below based on exposure at 100 kV for doses from 5 to 120 µC/cm<sup>2</sup>. The dose clear is dependent on softbake temperature, in this case 200C and 180C is used. Process parameters are:
A contrast curve for AR-P 617.06 is provided below based on exposure at 100 kV for doses from 5 to 120 µC/cm<sup>2</sup>. The dose to clear is dependent on softbake temperature, in this case 200C and 180C is used. Process parameters are:


*Date: February 5th 2024
*Date: February 5th 2024