==Deposition of Silicon using sputter deposition== | ==Deposition of Silicon using sputter deposition== | ||
At Nanolab you can | At Nanolab you can sputter silicon the using Wordentec or the Lesker Sputter systems. One of the advantages here is that you can deposit on almost any material you like. | ||
* [[Specific Process Knowledge/Thin film deposition/Si sputter in Wordentec|Si sputter deposition in the Wordentec]] | * [[Specific Process Knowledge/Thin film deposition/Si sputter in Wordentec|Si sputter deposition in the Wordentec]] | ||
* [[Specific Process Knowledge/Thin film deposition/Deposition of Silicon/Si sputter in Sputter-System Lesker|Si sputter deposition in the Sputter-System (Lesker)]] - ''includes information on surface roughness and stress'' | * [[Specific Process Knowledge/Thin film deposition/Deposition of Silicon/Si sputter in Sputter-System Lesker|Si sputter deposition in the Sputter-System (Lesker)]] - ''includes information on surface roughness and stress'' | ||
* [[Specific Process Knowledge/Thin film deposition/Deposition of Silicon/Si sputter in Sputter-System Metal-Oxide(PC1)|Si sputter deposition in the Sputter-System Metal-Oxide(PC1)]] | * [[Specific Process Knowledge/Thin film deposition/Deposition of Silicon/Si sputter in Sputter-System Metal-Oxide(PC1)|Si sputter deposition in the Sputter-System Metal-Oxide(PC1)]] | ||
* [[Specific Process Knowledge/Thin film deposition/Deposition of Silicon/Si sputter in Sputter-System Metal-Oxide(PC3)|Si sputter deposition in the Sputter-System Metal-Oxide(PC3)]] | * [[Specific Process Knowledge/Thin film deposition/Deposition of Silicon/Si sputter in Sputter-System Metal-Oxide(PC3)|Si sputter deposition in the Sputter-System Metal-Oxide(PC3)]] | ||
Historical note: It was previosly possible to sputter Si with our [[Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300| IonFab 300]]. You can read about the deposition conditions and results from that [[Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300/IBSD of Si|here]]. | |||
==Deposition of Silicon using PECVD== | ==Deposition of Silicon using PECVD== | ||
| Line 178: | Line 180: | ||
| | | | ||
|} | |} | ||
Revision as of 14:59, 22 January 2024
Feedback to this page: click here
Unless otherwise stated, this page is written by DTU Nanolab internal
PolySilicon can be deposited in several Nanolab tools. It can be sputtered, e-beam evaporated or be deposited in the PolySilicon furnaces. In the chart below you can compare the different deposition methods:
Deposition of PolySilicon using LPCVD
DTU Nanolab has two furnaces for deposition of LPCVD (Low Chemical Vapour Deposition) polysilicon: A 6" furnace (installed in 2011) for deposition of standard polySi, amorphous polySi and boron doped polySi on 100 mm or 150 mm wafers and a 4" furnace (installed in 1995) for deposition of standard polySi, amorphous polySi, boron- and phosphorous doped polySi on 100 mm wafers. In LabManager the two furnaces are named "Furnace: LPCVD Poly-Si (4") (B4)" and "Furnace: LPCVD Poly-Si (6") (E2)", respectively.
- Deposition of polysilicon using the 4" polysilicon furnace
- Deposition of polysilicon using the 6" polysilicon furnace
Deposition of Silicon using sputter deposition
At Nanolab you can sputter silicon the using Wordentec or the Lesker Sputter systems. One of the advantages here is that you can deposit on almost any material you like.
- Si sputter deposition in the Wordentec
- Si sputter deposition in the Sputter-System (Lesker) - includes information on surface roughness and stress
- Si sputter deposition in the Sputter-System Metal-Oxide(PC1)
- Si sputter deposition in the Sputter-System Metal-Oxide(PC3)
Historical note: It was previosly possible to sputter Si with our IonFab 300. You can read about the deposition conditions and results from that here.
Deposition of Silicon using PECVD
At Nanolab you can also deposit silicon the using PECVD. The deposition temperature is 300 °C.
Comparison of the methods for deposition of Silicon
| 4" and 6" Furnace PolySi (Furnace LPCVD PolySi) | PECVD (PECVD) | Sputter (Wordentec) | Sputter (Lesker) | Sputter (Sputter-system Metal-Oxide (PC1) and Sputter-system Metal-Nitride (PC3)) | |
|---|---|---|---|---|---|
| General description | LPCVD (low pressure chemical vapour deposition) of a-Si and poly-Si | Plasma Enhanced Chemical Vapor Deposition of Si | Sputter deposition of Si. | Sputter deposition of Si. | Sputter deposition of Si. |
| Doping facility | Yes, B (boron) and P (phosphorus) | Yes, B and P | None | None | None |
| Pre-clean | New wafers can go directly into the furnace. Processed wafers have to be RCA cleaned | RF Ar clean available | RF Ar clean available | RF Ar clean available | |
| Layer thickness | ~5 nm to 2 µm, if thicker layers are needed please ask the furnace team. | few nm to ~ 600 nm | few nm to ~ 300 nm | few nm to >200 nm | few nm to ? |
| Deposition rate |
|
~6 Å/s can probably be higher |
On the order of 1 Å/s dependent on process parameters. See more here. |
Depends on process parameters, roughly 0.2-2 Å/s. See Process Log. | Depends on process parameters, at least 0.3 Å/s, see conditions here |
| Process temperature | 560 °C (amorphous) and 620 °C (poly) | 300 °C | Wafers can be heated to 400 °C | Wafers can be heated to 600 °C | |
| Step coverage | Good | Medium | Medium | Medium | Medium - may be possible to improve using HIPIMS |
| Adhesion | Good for fused silica, silicon oxide, silicon nitride, silicon | Not tested, but do not deposit on top of silicon | |||
| Batch size |
|
|
|
|
|
| Allowed substrates |
|
|
|
|
|
| Allowed material | *Only those above (under allowed substrates). |
|
|
|
|
| Comment | Only in PECVD3 |