Specific Process Knowledge/Thermal Process/RTP Jipelec 2: Difference between revisions
Appearance
| Line 127: | Line 127: | ||
*Metals - ask for permisson | *Metals - ask for permisson | ||
*III-V materials - '''these cannot be heated above 450 °C,''' otherwise it can lead to outgassing of toxic gases. For that reason, '''III-V samples are limited to a maximum process temperature of 440 °C.''' | *III-V materials - '''these cannot be heated above 450 °C,''' otherwise it can lead to outgassing of toxic gases. For that reason, '''III-V samples are limited to a maximum process temperature of 440 °C.''' | ||
|style="background:WhiteSmoke; color:black;" align="left"| Always check the cross contamination information in LabManager to see whether your samples are allowed in the RTP2 Jipelec before using it. If you want to anneal sample materials that are not on the list or not approved, please contact the | |style="background:WhiteSmoke; color:black;" align="left"| Always check the cross contamination information in LabManager to see whether your samples are allowed in the RTP2 Jipelec before using it. If you want to anneal sample materials that are not on the list or not approved, please contact the Thin Film group | ||
|- | |- | ||
|} | |} | ||