Specific Process Knowledge/Lithography/EBeamLithography/BEAMER: Difference between revisions
Appearance
| Line 109: | Line 109: | ||
''Feature Sorting in Field:'' Can be used to alter the writing order of pattern elements in each writing field. The actual result of these choices can be somewhat hard to predict. After export the result can be seen in the Viewer under ''Tool'' and either ''Show Traversal Path'' or ''Show Writing Order''. | ''Feature Sorting in Field:'' Can be used to alter the writing order of pattern elements in each writing field. The actual result of these choices can be somewhat hard to predict. After export the result can be seen in the Viewer under ''Tool'' and either ''Show Traversal Path'' or ''Show Writing Order''. | ||
'''Important notice:''' If using the ''Fracture'' node to define the fracturing it is important in the ''Export'' node to explicitly choose not to fracture the layout during export. To ensure this select ''Cell To Field'' in the ''Field Ordering'' menu and ''NoCompaction'' in the ''Feature Sorting in Field'' of the export node. | |||
{| style="border: none; border-spacing: 0; margin: 1em auto; text-align: center;" | {| style="border: none; border-spacing: 0; margin: 1em auto; text-align: center;" | ||
| Line 117: | Line 118: | ||
JEOL V30 version of the Beamer export node. | JEOL V30 version of the Beamer export node. | ||
|} | |} | ||
===Extract=== | ===Extract=== | ||