Specific Process Knowledge/Lithography/EBeamLithography/BEAMER: Difference between revisions
Appearance
| Line 113: | Line 113: | ||
| colspan="3" style="text-align:center;| | | colspan="3" style="text-align:center;| | ||
?. | ?. | ||
|} | |||
===Extract node=== | |||
The extract node allows one to extract only parts of a design for further processing and export. The available options are: | |||
''Layer(s):'' Extract single or multiple layers from the design file. | |||
''Extraction type:'' Allows extraction of single cells of a design or a drawn region. In the example shown below a region has been drawn in the viewer by simply Shift-left clicking to select the region. The corners of a region can also be entered nummerically. Multiple regions can be defined for extraction. By clicking the ''Exclude Region(s)/Instance'' the selected parts can be omitted from the rest of the pattern instead. | |||
''Dose Classification:'' The dose modulation table (if any is present from PEC) can be truncated with the ''Shrink'' option to reflect the extracted region. | |||
On the ''Extent'' pane one has the option to control the bounding box of the extracted geometry. | |||
{| style="border: none; border-spacing: 0; margin: 1em auto; text-align: center;" | |||
|- | |||
| [[image:BEAMER_Extract.png|600px]] | |||
|- | |||
| colspan="1" style="text-align:center;| | |||
Beamer extract node. | |||
|} | |} | ||