We will spend the coming weeks on the installation and acceptance tests of the tool and prepare the training protocol.  
We will spend the coming weeks on the installation and acceptance tests of the tool and prepare the training protocol.  
We hope that you will receive the tool well when we release it, which we expect to do in September.
We hope that you will receive the tool well when we release it, which we expect to do in September.
The image shows a freshly cleaved cross section of a mulilayered thin film of alternating layers of 5 nm TiO2 and 5 nm Al2O3 deposited by ALD.