Specific Process Knowledge/Etch/DRIE-Pegasus/Pegasus-4/SiO2 Etch: Difference between revisions

Bghe (talk | contribs)
Bghe (talk | contribs)
Line 60: Line 60:


==Testing with electromagnetic coils==
==Testing with electromagnetic coils==
===by bghe@nanolab 2023===<br>
''by bghe@nanolab 2023'' <br>


When testing with decreased platen power on the SiO2_10 standard recipe the uniformity got very bad. I then tested with the electromagnetics coil to see if that could affect the uniformity. There is and outer coil that can be varied between 0 and 10A and an inner coil that can be varied between 0 and 30 A. The first tests were don on Si/SiO2(1µm) without pattern and measured on the ellipsometer.  
When testing with decreased platen power on the SiO2_10 standard recipe the uniformity got very bad. I then tested with the electromagnetics coil to see if that could affect the uniformity. There is and outer coil that can be varied between 0 and 10A and an inner coil that can be varied between 0 and 30 A. The first tests were don on Si/SiO2(1µm) without pattern and measured on the ellipsometer.