Specific Process Knowledge/Thermal Process/RTP Annealsys: Difference between revisions

Indiogo (talk | contribs)
Indiogo (talk | contribs)
Line 9: Line 9:
''January 2023: The RTP Annealsys is being tested, but it is not released for general use yet. Please contact thinfilm@nanolab.dtu.dk for more information.''
''January 2023: The RTP Annealsys is being tested, but it is not released for general use yet. Please contact thinfilm@nanolab.dtu.dk for more information.''


'''RTP Annealsys (RTP AS-Premium, serial number AS0415C4 -  8177, from ANNEALSYS)''' is a research tool available at DTU Nanolab that can reach very high temperatures in a matter of a few minutes or even seconds. Therefore, it is able to perform several types of rapid thermal processing and it can be used as a multi-functional and versatile microfabrication tool, within specific process windows for each process type, using Si/nanofabricated Si structures. Amongst them, there is rapid thermal annealing '''(RTA)''', hydrogenation '''(RTH)''', oxidation '''(RTO)''', nitridation '''(RTN)''', etc. Currently, it is used for '''rapid thermal annealing and smoothing''' of silicon-based samples.
'''RTP Annealsys (RTP AS-Premium, serial number AS0415C4 -  8177, from ANNEALSYS)''' is a research tool available at DTU Nanolab that can reach very high temperatures in just a few minutes or even seconds. Therefore, it is able to perform several types of rapid thermal processing and it can be used as a multi-functional and versatile microfabrication tool, within specific process windows for each process type, using Si/nanofabricated Si structures. Amongst them, there are rapid thermal annealing '''(RTA)''', hydrogenation '''(RTH)''', oxidation '''(RTO)''', nitridation '''(RTN)''', etc. Currently, it is used for '''rapid thermal annealing and smoothing''' of silicon-based samples.


[[File:LL&station Annealsys.png|450px|thumb|right|The RTP Annealsys work station and loadlock are located in the DTU Nanolab cleanroom B-1. Photo: Maria Farinha@DTU Nanolab, February 2023]]
[[File:LL&station Annealsys.png|450px|thumb|right|The RTP Annealsys work station and loadlock are located in the DTU Nanolab cleanroom B-1. Photo: Maria Farinha@DTU Nanolab, February 2023]]