Jump to content

Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300/Crystal Settings: Difference between revisions

From LabAdviser
Bghe (talk | contribs)
No edit summary
Bghe (talk | contribs)
No edit summary
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/IBE⁄IBSD_Ionfab_300/Crystal_Settings click here]'''  
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/IBE⁄IBSD_Ionfab_300/Crystal_Settings click here]'''  
===As the system is not being used for deposition this information is no long relevant===
It is being keep in case we will start up the depostion again.<br>


<!-- [[Image:Tooling_factor.jpg|700px|right|thumb|How to calculate the tooling factor. Taken from the manufacture manual]] -->
<!-- [[Image:Tooling_factor.jpg|700px|right|thumb|How to calculate the tooling factor. Taken from the manufacture manual]] -->

Revision as of 14:58, 22 June 2023

Feedback to this page: click here

As the system is not being used for deposition this information is no long relevant

It is being keep in case we will start up the depostion again.


Material parameters for using the crystal monitors
Material Density Z ratio
TiO2 4.260 0.400
SiO2 2.648 1.000
Si 2.320 0.712


Settings for Crystal thickness monitor 1
Date Tooling factor: TiO2 Tooling factor: SiO2 Tooling factor: Si
2014-07-22 157.3% (wafer center)
2015-09-08 132 % B2 B3
C C1 C2 C3
D D1 D2 D3


Settings for crystal thickness monitor 2
Date Tooling factor: TiO2 Tooling factor: SiO2 Tooling factor: Si
A A1 A2 A3
B B1 B2 B3
C C1 C2 C3
D D1 D2 D3