'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_ZnO click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_ZnO click here]''' | ||
<i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i> | |||
ZnO can be deposited by Sputtering process and atomic layer deposition (ALD). In the chart below you can compare the different deposition equipment. | ZnO can be deposited by Sputtering process and atomic layer deposition (ALD). In the chart below you can compare the different deposition equipment. | ||
Revision as of 14:55, 6 June 2023
Feedback to this page: click here
Unless otherwise stated, this page is written by DTU Nanolab internal
ZnO can be deposited by Sputtering process and atomic layer deposition (ALD). In the chart below you can compare the different deposition equipment.
| Sputtering deposition (Lesker) | Atomic layer deposition (ALD Picosun R200) | |
|---|---|---|
| General description | Sputter deposition of ZnO | Atomic layer deposition of ZnO |
| Pre-clean | RF Ar clean | |
| Layer thickness | 10Å to 5000Å* | 0 to 1000 Å |
| Deposition rate | Depending on process parameters. | Depending on temperature |
| Batch size |
|
|
| Allowed materials |
|
|
| Comment |
|
* For thicknesses above 200 nm permission is required.