'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/XRD/HighScore_analysis click here]''' | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/XRD/HighScore_analysis click here]''' | ||
<i> | <i> This page is written by <b>DTU Nanolab internal</b></i> | ||
Revision as of 13:48, 11 May 2023
Feedback to this page: click here
This page is written by DTU Nanolab internal
HighScore Plus
HighScore Plus is the software package supplied with the Malvern Panalytical Aeris benchtop Powder XRD. This software is available on the shared data analysis computer located in 346-904 just to the right of the XRD Powder. You can log onto this computer either directly when you are sitting in front of it or through remote desktop from your own computer. For more details on how to login remotely, please see this note in LabManager - requires login.
Using HighScore Plus
For a guide to use this software, we recommend that users try to follow the tutorial found on LabManager - requires login.
HighScore Plus has several analysis functions for which there is no license in SmartLab Studio II, including Structure Solution, Structure Refinement, and Rietveld analysis. The software is only suitable for powder analysis.