Specific Process Knowledge/Lithography/EBeamLithography/FilePreparation/Pathlist: Difference between revisions
Appearance
| Line 1: | Line 1: | ||
=Path list= | =Path list= | ||
This is the full path list as available on the JEOL 9500 system. Please contact the EBL staff if you need a custom path defined on the tool. <div class=" | This is the full path list as available on the JEOL 9500 system. Please contact the EBL staff if you need a custom path defined on the tool. <div class="left" style="color:red; width:auto; margin-left:auto; margin-right:auto;">'''Users are NOT allowed to change the path definition file on the system.'''</div> | ||
<pre> | <pre> | ||
Revision as of 17:38, 16 April 2023
Path list
This is the full path list as available on the JEOL 9500 system. Please contact the EBL staff if you need a custom path defined on the tool.
Users are NOT allowed to change the path definition file on the system.
;;*** Mask Exposure Peformance Test ***
MASK00: INITIAL HEIMAP,CURRNT,INITBE,PDEFBE,DISTBE,PDEFBE,SUBDEFBE
CYCLIC CURRNT,DRIFT
CYCLE 5M
MASK01: INITIAL HEIMAP,CURRNT,INITBE,PDEFBE,SUBDEFBE
CYCLIC CURRNT,DRIFT
CYCLE 5M
;;*** Direct Exposure Peformance Test ***
DIRE00: INITIAL CURRNT,INITBE,PDEFBE,DISTBE,PDEFBE,SUBDEFBE
CYCLIC CURRNT
CYCLE 5M
DIRE01: INITIAL CURRNT,INITBE,PDEFBE,SUBDEFBE
CYCLIC CURRNT
CYCLE 5M
;;*** Minimum Line Exposure Peformance Test ***
MINI01: INITIAL CURRNT,INITBE,PDEFBE,SUBDEFBE
CYCLIC CURRNT,DRIFT
CYCLE 5M
;;*** Test Exposure ***
TEST00: INITIAL HEIMAP
TEST01: INITIAL CURRNT
TEST02: INITIAL HEIMAP,CURRNT
TEST03: INITIAL CURRNT,INITBE
TEST04: INITIAL HEIMAP,CURRNT,INITBE
TEST05: INITIAL CURRNT,INITBE,PDEFBE,SUBDEFBE
TEST06: INITIAL HEIMAP,CURRNT,INITBE,PDEFBE,SUBDEFBE
TEST07: INITIAL CURRNT,INITBE,PDEFBE,DISTBE,SUBDEFBE
TEST08: INITIAL HEIMAP,CURRNT,INITBE,PDEFBE,DISTBE,SUBDEFBE
TEST09: INITIAL CURRNT,INITBE,PDEFBE,SUBDEFBE
CYCLIC CURRNT,DRIFT
CYCLE 1
TEST10: INITIAL HEIMAP,CURRNT,INITBE,PDEFBE,SUBDEFBE
CYCLIC CURRNT,DRIFT
CYCLE 1
TEST11: INITIAL CURRNT,INITBE,PDEFBE,DISTBE,SUBDEFBE
CYCLIC CURRNT,DRIFT
CYCLE 5M, F
TEST12: INITIAL HEIMAP,CURRNT,INITBE,PDEFBE,DISTBE,SUBDEFBE
CYCLIC CURRNT,DRIFT
CYCLE 5M, F
TEST13: INITIAL INITAE,INITBE,CURRNT,PDEFBE
CYCLIC DRIFT
CYCLE 1M, F
TEST14: INITIAL CURRNT
CYCLIC DRIFT
CYCLE 99
DRIFT0: INITIAL INITAE, INITBE
CYCLIC INITAE, INITBE, DRIFT, CURRNT
CYCLE 1
DRIFT1: INITIAL INITAE, INITBE
CYCLIC INITAE, INITBE, DRIFT, CURRNT
CYCLE 1M,F
LONG01: INITIAL CURRNT,INITBE,PDEFBE,DISTBE,SUBDEFBE
CYCLIC CURRNT,DRIFT
CYCLE 5M
LONG02: INITIAL CURRNT,INITBE,PDEFBE,SUBDEFBE
CYCLIC CURRNT,DRIFT,INITBE,PDEFBE,SUBDEFBE
CYCLE 5M
MINI02: INITIAL CURRNT,INITBE,PDEFBE,SUBDEFBE
CYCLIC CURRNT,INITBE
CYCLE 20M
HEIGH1: INITIAL HEIMAP,CURRNT
CYCLIC CURRNT,DRIFT
CYCLE 10M
MASK02: INITIAL CURRNT,INITBE,PDEFBE,SUBDEFBE
CYCLIC DRIFT,CURRNT
CYCLE 4
MASK03: INITIAL CURRNT,INITBE,PDEFBE,SUBDEFBE
CYCLIC CURRNT,DRIFT
CYCLE 5M
MASK04: INITIAL CURRNT,INITBE,PDEFBE,DISTBE,PDEFBE,SUBDEFBE
CYCLIC CURRNT,DRIFT
CYCLE 5M
MASK05: INITIAL HEIMAP,CURRNT,INITBE,PDEFBE,DISTBE,SUBDEFBE
CYCLIC CURRNT,DRIFT
CYCLE 5M
MASK06: INITIAL CURRNT,INITBE,PDEFBE,SUBDEFBE
CYCLIC INITBE,PDEFBE,SUBDEFBE,CURRNT,DRIFT
CYCLE 5M
AUTO00: INITIAL CURRNT,INITBE,PDEFBE,DISTBE,PDEFBE,SUBDEFBE
DIRE02: INITIAL CURRNT,INITBE,PDEFBE,SUBDEFBE
DIRE03: INITIAL CURRNT,INITBE
CYCLIC CURRNT,DRIFT
CYCLE 20M
DIRE04: INITIAL CURRNT,INITBE,PDEFBE
CYCLIC CURRNT
CYCLE 20M
DIRE05: INITIAL CURRNT,INITBE,PDEFBE,SUBDEFBE
CYCLIC CURRNT
CYCLE 20M
DIRE06: INITIAL CURRNT,INITBE,PDEFBE,DISTBE,SUBDEFBE
CYCLIC CURRNT
CYCLE 20M
DIRE07: INITIAL CURRNT,INITBE,PDEFBE,DISTBE,PDEFBE,SUBDEFBE
CYCLIC CURRNT
CYCLE 20M
DRFT01: INITIAL CURRNT
CYCLIC DRIFT
CYCLE 1
SBG01: INITIAL HEIMAP,CURRNT,INITBE,PDEFBE,SUBDEFBE
SBG02: INITIAL HEIMAP
SBG03: INITIAL CURRNT,INITBE,PDEFBE,SUBDEFBE
CYCLIC CURRNT,DRIFT
CYCLE 5M
SBG04: INITIAL CURRNT,INITBE,PDEFBE,SUBDEFBE
CYCLIC CURRNT,DRIFT
CYCLE 5M
SBG05: INITIAL CURRNT
CYCLIC CURRNT,DRIFT
CYCLE 5M
SBG06: INITIAL HEIMAP
CYCLIC CURRNT,DRIFT
CYCLE 5M
SBG07: INITIAL CURRNT
CYCLIC CURRNT,DRIFT
CYCLE 34
TOK01: INITIAL CURRNT,INITBE,PDEFBE,SUBDEFBE
CYCLIC CURRNT,DRIFT
CYCLE 20M
G5MHA: INITIAL HEIMAP
CYCLIC CURRNT,DRIFT
CYCLE 5M
G5MHB: INITIAL HEIMAP
CYCLIC DRIFT
CYCLE 5M
G5MA: INITIAL CURRNT
CYCLIC CURRNT,DRIFT
CYCLE 5M
G5MB: INITIAL CURRNT
CYCLIC DRIFT
CYCLE 5M
G34HA: INITIAL HEIMAP
CYCLIC CURRNT,DRIFT
CYCLE 34
G34HB: INITIAL HEIMAP
CYCLIC DRIFT
CYCLE 34
G34A: INITIAL CURRNT
CYCLIC CURRNT,DRIFT
CYCLE 34
G34B: INITIAL CURRNT
CYCLIC DRIFT
CYCLE 34
G1HA: INITIAL HEIMAP
CYCLIC CURRNT,DRIFT
CYCLE 1
G1HB: INITIAL HEIMAP
CYCLIC DRIFT
CYCLE 1
G1A: INITIAL CURRNT
CYCLIC CURRNT,DRIFT
CYCLE 1
G1B: INITIAL CURRNT
CYCLIC DRIFT
CYCLE 1
HEICU: INITIAL HEIMAP,CURRNT
HCD: INITIAL HEIMAP
CYCLIC CURRNT,DRIFT
CYCLE 30M
CD: INITIAL CURRNT
CYCLIC DRIFT
CYCLE 30M
FT01: INITIAL CURRNT
CYCLIC CURRNT,DRIFT
CYCLE 5M,F
LONG03: INITIAL CURRNT,INITBE,PDEFBE,SUBDEFBE
CYCLIC CURRNT,DRIFT,INITBE,PDEFBE,SUBDEFBE
CYCLE 5M,F
HEI: INITIAL HEIMAP
CYCLIC CURRNT
CYCLE 10M
DRF5M: INITIAL CURRNT,HEIMAP
CYCLIC CURRNT,DRIFT
CYCLE 5M,F
DTU5M: INITIAL HEIMAP,CURRNT,INITBE,PDEFBE,SUBDEFBE
CYCLIC CURRNT,DRIFT
CYCLE 5M,F
CUR: INITIAL CURRNT
CYCLIC CURRNT
CYCLE 30M