== User resist bottles in the cleanroom ==
== User resist bottles in the cleanroom ==


[[File:bottle.jpg|160px|thumb|right]]
[[File:bottle.jpg|320px|thumb|right]]


We recommend all e-beam users, and certain UV users, to have their own small bottle of resist inside the cleanroom.
We recommend all e-beam users, and certain UV users, to have their own small bottle of resist inside the cleanroom.