'''Procedure for bringing new user resist bottles into the cleanroom:''' | '''Procedure for bringing new user resist bottles into the cleanroom:''' | ||
#''Outside the cleanroom'': Find a blue-cap glass bottle in the | #''Outside the cleanroom'': Find a blue-cap glass bottle in the storage cabinet, next to office 055, in building 346 | ||
#''Gowning'': Clean the bottle in gowning | #''Gowning'': Clean the bottle in gowning | ||
#*Clean it thoroughly on the outside with water or alcohol | #*Clean it thoroughly on the outside with water or alcohol | ||